Printing Parameters
Nozzle Temperature: 200–240°C
Bed Temperature: 35–55°C
Bed Modification: PEI frosted board
Active Cooling Fan: ON, 50–100%
Layer Height: 0.2 mm
Shell Thickness: ≥ 0.8 mm
Print Speed: ≤ 200 mm/s
Note: Settings are based on a 0.4mm nozzle.
Description
100°C High Heat Deflection (HDT) Pushes PLA performance boundaries with a Vicat softening temperature elevated up to 100°C, dramatically eliminating heat creep and early softening in the hotend.
Upgraded Mechanical Strength Delivers superior impact resistance, tensile strength, and toughness compared to standard PLA, making it capable of replacing engineering materials for specific applications.
Smooth & Jam-Free Printing Engineered to eliminate premature melting in the cold zone, ensuring ultra-smooth extrusion, consistent flow, and reliable long-duration prints.
Professional-Grade Print Quality Combines the hassle-free printability of traditional PLA with exceptional dimensional accuracy and crisp surface detail.
Vibrant & Colorful Palette Available in a wide range of rich, colorful options to cater to both aesthetic creations and functional prototypes.
Technical Datasheet
Melt Temperature: ~160°C (ISO 11357)
Glass Transition Temperature: ~60°C (ISO 11357)
Melt Flow Rate (MFR): 15–20 g/10min¹ (ISO 1133)
Heat Deflection Temperature (HDT): 51°C² (ISO 75)
Vicat Softening Temperature (VST): 71°C³ (ISO 306)
Density: 1.24–1.26 g/cm³ (ISO 1183)
Odor: Odorless
Solubility: Insoluble in water
Note: ¹ Test conditions: T= 190℃; m= 2.16kg. ² Test conditions: 0.45MPa; 120℃/h. ³ Test conditions: 10N; 120℃/h.