Printing Parameters
Nozzle Temperature: 240–250°C
Bed Temperature: 35–55°C
Bed Modification: PEI frosted board
Active Cooling Fan: ON, 50–100%
Layer Height: 0.2 mm
Shell Thickness: ≥ 0.8 mm
Print Speed: 20 mm/s
Note: Settings are based on a 0.4mm nozzle.
Description
Balanced Softness & Integrity: Low-Shore 65A durometer offers superior flexibility with added structural shape retention over 60A.
Enhanced Soft-Flex Printability: Engineered for reliable feeding and smooth extrusion compared to softer flex materials.
High Elongation & Smooth Surface: Delivers high stretch capacity and a refined finish for premium tactile applications.
UV & Chemical Protection: UV-stabilized to resist sun damage, combined with high resistance to oils, greases, and abrasion
Technical Datasheet
Melt Flow Rate (MFR): 25–35 g/10min¹ (ISO 1133)
Heat Deflection Temperature (HDT): N/A² (ISO 75)
Vicat Softening Temperature (VST): N/A (ISO 306)
Density: 1.20–1.22 g/cm³ (ISO 1183)
Hardness: 62A (GB/T 531.1)
Resilience: 65% (GB/T 1681-2009)
Odor: Odorless
Solubility: Insoluble in water
Note: ¹ Test conditions: T= 210℃; m= 2.16kg. ² Test conditions: 0.45MPa; 130℃/h.
Applications